Leave Your Message
News Categories
Featured News

CF8M Stainless Steel Valve Body Casting for NPS 42" Class 300 Ball Valve

2026-05-24

NPS 42” CF8M Steel Valve Body Casting (Sand Casting, EAF Melted, RT Critical Areas, PT 100%, 4000 kg)

Telida Metals has successfully completed a large-scale NPS 42” valve body casting in CF8M stainless steel, manufactured for critical industrial pressure applications.

The casting was produced using a sand casting process, with a finished weight of approximately 4,000 kg, requiring strict control of solidification behavior, internal soundness, and non-destructive examination compliance for heavy-section stainless steel components.


🏭 Melting Process: Electric Arc Furnace (EAF)

The molten steel was produced via Electric Arc Furnace (EAF) melting, ensuring controlled refining of CF8M stainless steel chemistry.

This process supports:

  • Stable chromium and molybdenum distribution
  • Low inclusion content for pressure boundary integrity
  • Consistent corrosion resistance for aggressive service conditions

⚙️ Material: CF8M Austenitic Stainless Steel

The casting material is CF8M stainless steel, widely used in:

  • Oil & gas pressure systems
  • Chemical processing valves
  • Seawater and chloride environments
  • Large-diameter industrial flow control systems

CF8M provides high corrosion resistance and stable mechanical performance under pressure service conditions.


🧱 Manufacturing Process: Sand Casting (Large Valve Body)

Due to the geometry and mass of the component, a precision sand casting process was applied.

Key process controls included:

  • Mold design optimization for NPS 42” geometry
  • Controlled pouring sequence for thick-section filling stability
  • Shrinkage compensation for heavy-section solidification
  • Thermal control to minimize internal discontinuities

🔬 Non-Destructive Examination (NDE) Compliance

✔ Liquid Penetrant Testing (PT) — 100% Coverage

All accessible surfaces were subjected to 100% Liquid Penetrant Testing (PT) in accordance with:

ASME BPVC Section VIII, Division 1 — Mandatory Appendix 8

PT inspection was applied to detect surface-breaking discontinuities such as:

  • Surface porosity
  • Hot tears
  • Cracks
  • Surface shrinkage indications

Acceptance evaluation was performed strictly according to Appendix 8 criteria.


✔ Radiographic Testing (RT) — Critical Area Coverage

Radiographic Testing (RT) was performed on critical casting areas, including:

  • Section transitions with abrupt geometry changes
  • Junctions of risers, gates, and feeders
  • Areas with highest solidification stress concentration

RT execution followed:

ASME BPVC Section V — Article 2 (Radiographic Examination)
Acceptance criteria: ASME BPVC Section VIII, Division 1 — Mandatory Appendix 7

Critical evaluation was focused on:

  • Internal shrinkage
  • Gas porosity
  • Slag inclusions
  • Density-related discontinuities in heavy sections

⚠ Critical Engineering Interpretation (Code Alignment)

According to ASME BPVC VIII Appendix 7, inspection severity is not based solely on flaw existence, but on:

“Severity level of imperfections in relation to casting thickness and service category.”

For large-section castings such as NPS 42”, inspection rigor is concentrated on:

  • High-stress geometric transitions
  • Feeding and solidification zones
  • Pressure boundary integrity regions

⚖ Product Scale & Engineering Complexity

This project represents a high-integrity industrial casting:

  • Nominal size: NPS 42”
  • Material: CF8M stainless steel
  • Casting weight: ~4000 kg
  • Process route: EAF melting → sand casting → controlled cooling → PT 100% → RT critical areas

The combination of large thermal mass + stainless steel + pressure boundary application requires strict adherence to ASME nondestructive examination standards.


🏁 Application

The component is intended for critical industrial valve systems, where long-term reliability depends on:

  • Internal soundness (RT verified zones)
  • Surface integrity (PT 100%)
  • Material corrosion resistance (CF8M)